Packaging | as per request |
The cores of MSB series are made of thin (18 +-2 microns) Co-based amorphous ribbon, have square B-H loop and have much higher permeability than their analogs made of Fe-Ni-based permalloys and ferrites.
The product's design is optimized for use with single-turn coil, which is usually component (transistor, diode) output.
KEY FEATURES OF THE AMORPHOUS MATERIAL:
· Induction amplitude, Bm (25°C) 0.62 T
· Induction amplitude, Bm (90°C) 0.54 T
· Squareness ratio Br/Bm (@ 100 kHz, 80 A/m) at least 0.90
· Curie temperature, Tc 225°C
· Operating temperature range -60°C ... +100°C
· Magnetostriction less than 0.1´10^-6
CONFIGURATION:
Ribbon wound magnetic core is placed into hard protective container of glass-polyamide and mechanically fixed with silicone sealant. The container provides reliable mechanical protection and preservation of amorphous material's properties. All materials comply with UL94V-1 / 0.
0.DIMENSIONS AND KEY FEATURES:
TYPEDimensions in container (without a container)
(mm)
Mean line length
Lm, mm
Cross-section
Ac, mm2
Inductance
AL
(µH/turn2)
(50 kHz)
Dynamic parameters
@ F=100 kHz, Hm=1 Oe (80 A/m), 25°C
Flux
2Фm
(µWb)
Coercitivity
Hc
(A/m)
Squareness ratio
Br/Bm
(%)
Nominal Nominal Nominal Min Max MinMSB– 03A - N |
4.0-1.5-4.5 (3.0-2.0-3.0) |
7.75 | 1.20 | 3.00 | 1.10 | 25 | 88 |
MSB – 03S - N |
4.0-1.5-6.0 (3.0-2.0-4.5) |
7.75 | 1.80 | 5.00 | 1.65 | ||
MSB – 03B - N |
4-1.5-7.5 (3.0-2.0-6.0) |
7.85 | 2.40 | 7.00 | 2.20 | ||
MSB – 04S - N |
5.1-1,5-6.0 (4.0-2.0-4.5) |
9.06 | 3.60 | 9.00 | 3.30 | ||
MSB – 04B - N |
5.1-1.5-7.5 (4.0-2.0-6.0) |
9.06 | 4.80 | 12.0 | 4.40 | ||
MSB-045A-N |
6.5-2.4-6.0 (4.5-4.0-3.0) |
13.30 | 0.59 | 0.89 | 0.62 | ||
MSB-05A-N |
7.0-2.4-6.0 (5.0-4.0-3.0) |
14.10 | 1.17 | 1.40 | 1.05 | ||
Operating temperature range -60°C ... +100°C |