Place of Origin | Jiangsu, China | Type | Nickel Bar |
Application | widely, in air plane, oil | Grade | inconel 625 |
Ni (Min) | 68% | Resistance (u03bcu03a9.m) | standard |
Powder Or Not | Not Powder | Ultimate Strength (u2265 MPa) | 965 |
Elongation (u2265 %) | 30 | Model Number | inconel 625 |
Brand Name | Raymond |