Place of Origin | Shanxi, China | Model Number | 4000m |
Type | Powder | Weight | -- |
Technique | Washed Kaolin | Dimensions | Washed |
SiO2 Content (%) | 56 | Fe2O3 Content (%) | 0.25±0.1 |
Al2O3 Content (%) | 46±1 | Moisture Content (%) | 0.2 |
TiO2 Content (%) | 0.1 | K2O Content (%) | 0.05 |
Application | REFRACTORY | Product name | calcined kaolin |
Usage | paint | Shape | Power |
Usage2 | paper | Feature | improve coating covering power |
Feature2 | weathering resistance |