Please wait while your account is being registered at Tradewheel.com Loading Spinner

Join World's Fastest Growing B2B Network

Parallel Twin Screw Barrel Double Screw Barrel for PVC Pelletizing

FOB Price 1 - 50 USD / pieces

Quick Details (View All)

Model NO.Twin Parallel Screw Barrel ScrewTwin-Screw
Engagement SystemFull Intermeshing Screw Channel StructureDeep Screw
AutomationAutomatic ComputerizedComputerized
Transport PackageWooden Case SpecificationISO9001: 2008
TrademarkZhongyang OriginZhoushan
HS Code84779000 Production Capacity1500sets/Month

Product Details

Product Description

Parallel Twin Screw Barrel for PVC Pelletizer pelletizing screw barrel, PVC extrusion screw barrel, plastic machinery screw barrel

Specification:
Diameter: Φ 45mm-Φ 200mm
L/D ratio: 16-35
The compression ratio of screws can be designed according to different products and ingredients

Technical Information

Base Materials:
1)38CrMoAlA(JIS SACM645)
2)42CrMo(AISI 4140)
3)4Cr5MoSi V1 (JIS SKD-61)
4)9Cr18MOV
5)HPT

Bimetallic alloy materials:
1)Fe-based alloy
2)Ni-based alloy/Deloro alloy
3)Co-based alloy
4)NiCo-based alloy
5)Tungsten carbide/Wolfram carbide

Technics:
Heat treatment
High-frequency quenching
Nitriding treatment
Hard-chrome electroplating
Bimetallic alloy welding
Bimetallic alloy centrifugal casting

Technical parameter:
Nitrided layer depth: 0.5-0.8mm
Nitrided hardness: 900-1000HV
Nitrided brittleness: Less than grade 1
Surface roughness: Ra0.4
Linearity of screw: 0.015mm
Hard-chrome plating hardness after nitriding: >=950HV
Chrome-plating layer depth: 0.025-0.085mm
Bimetallic layer depth: 3mm

Warranty and service: 1 year

Our advantages:
1)Excellent raw materials
2)Good customer service
3)Rapid delivery
4)Reasonable price
5)Production quickly

Experienced manufacture, we will be the best choice.
Main Base materials
1.38CrMoAlA (Nitriding Steel)
2. SKD-61 (Special Tool Steel)
3. 42CrMo (Ultrahigh Strength Steel)
4. DC53 ( Cold Work Die Steel)
5. W6Mo5Cr4V2 ( High-Speed Tool Steel )
6. HPT


Main Alloy Materials
1. Ni-based alloy/Deloro alloy
2. Tungsten carbide/Wolfram carbide
3. NiCo-based alloy
4. Fe-based alloy
5. Co-based alloy



Processing Technics
1. Heat treatment
2. Quenching
3. Nitriding treatment
4. Bimetallic alloy welding
5. Bimetallic alloy centrifugal casting
6. Hard-chrome electroplating




Technical parameters
Nitriding layer depth 0.5-0.8mm
Nitrided hardness HRC56-58
Nitrided brittleness Less than grade 1
Surface roughness Ra 0.4
Linearity of screw 0.015mm
Hard-chrome plating hardness ≥HRC57
Chrome-plating layer depth 0.03-0.09mm
Bimetallic layer depth 3 mm
Bimetallic layer hardness HRC58-62