Thickness | 0.01mm - 0.8mm |
1.Overview:
Standard beryllium copper alloys contain close to 2% beryllium, while the beryllium content in proprietary alloys can range from 1.5% to 2.7%. In its age hardened condition, beryllium copper attains the highest strength and hardness of any commercial copper-based alloy.
We focus on the production of beryllium copper strips of various sizes, including C17200 and C17410. The beryllium in C17200 strip is 1.8% - 2.0% while C17410 contains 0.15% - 0.5% of beryllium. The Thickness of our products ranges from 0.01MM to 0.8MM.
2. C17200 Typical Physical Properties*
Elastic modulus |
Melting Point (Solidus) |
Electrical Conductivity | Density** |
Thermal Expansion Coefficient (20 °C to 200 °C) |
Thermal Conductivity (25 °C) |
130 Gpa | 870 °C | 20-25% IACS | 8.36 g/cm3 | 17.3x10-6 m/m °C | 110W/mK |
*Properties listed for the precipitation age hardened (heat
treated) condition. **Density in the cold-rolled condition (prior to heat treatment) is 8.36g/cm3 |
3. C17410 Metalic Properties
Designation. |
Status |
HV |
0.2% Yield strength |
Tensile
strength |
Min.
|
Min.
|
C17410 |
TH02 |
180 ~ 230 |
550 ~ 690 |
665 ~ 790 |
≥ 45 |
10 ~ 20 |
TH04 |
210 ~ 278 |
690 ~ 830 |
760 ~ 895 |
≥ 45 |
7 ~ 17 |