MOQ | 100 KG |
Port | SHANGHAI |
Packaging | 1,5,15KG |
Lead Time | 25days |
Technical date sheet NI ALLOY WELDING WIRE
Ni base alloy solid welding wire for welding which has excellent cracking resistance to ductility dip cracking in weld metal, can increase the tensile strength of the weld metal to not less than the tensile strength of the base material, and has excellent weld ability.
AWS A5.4 |
ERNi-1 |
ERNiCu-7 |
ERNiCr-3 |
ERNiCrFe-5 |
ERNiCrMo-3 |
ERNiCrMo-4 |
ERNiFeCr-1 |
Tensile
Strength |
514 |
541 |
671 |
651 |
819 |
729 |
602 |
Elongation |
44 |
39 |
41 |
45 |
39 |
45 |
33 |
C |
0.02 |
0.02 |
0.03 |
0.06 |
0.037 |
0.012 |
0.02 |
Mn |
0.24 |
3.21 |
3.05 |
0.51 |
0.06 |
0.5 |
0.5 |
Si |
0.34 |
0.68 |
0.12 |
0.14 |
0.11 |
0.01 |
0.11 |
P |
0.34 |
1.53 |
2.4 |
1.99 |
3.37 |
0.23 |
0.81 |
Ti |
0.34 |
1.53 |
/ |
/ |
/ |
/ |
0.81 |
S |
0.14 |
0.47 |
1.41 |
6.82 |
3.9 |
5.4 |
28.24 |
Cr |
/ |
/ |
19.86 |
14.79 |
21.55 |
15.9 |
22.61 |
Ni |
95.5 |
65.68 |
72.8 |
75.06 |
61.65 |
REM |
42.91 |
Cu |
0.01 |
REM |
0.03 |
0.03 |
/ |
/ |
/ |
Mo |
0.01 |
REM |
0.03 |
0.03 |
8.49 |
16 |
2.67 |
Nb |
/ |
|
2.4 |
1.99 |
3.37 |
/ |
|
V |
/ |
|
|
|
|
0.23 |
|
Fe |
0.14 |
0.47 |
1.41 |
6.82 |
3.9 |
5.4 |
28.24 |