MOQ | 5000 t |
Port | Vietnam |
Lead Time | 1 week |
OEM | Available | Color | Black |
Quality | Good | Chemical Formula | C |
(1) Partial replacement of metallurgical coke with pulverized coal reduces the blast furnace iron-to-coke ratio and pig iron cost;
(2) Adjusts the furnace condition heat system and stable operation;
(3) the injected pulverized coal is gasified and burned before the blast furnace tuyere to reduce the theoretical combustion degree. Compensation is required, which creates conditions for the blast furnace to use high air and oxygen-enriched blast;
(4) Injecting pulverized coal to replace part of the coke, on the one hand, can save coking investment, build less coke ovens, and reduce air pollution caused by coking.
Our Quality Report:
Aad: 12
Vad: 10
St,d: 0.8
HGI: 60
Qgr,ad: 6800
0-40mm: >90%
No.17A, Wanguguoji, Runcheng, Xishan district, Kunming city, Yunnan province